| Performance table of EPO foaming products | |||||||
| performance items | test standards | ||||||
| density | ASTM-D3575 | 1.25 | 1.50 | 1.75 | 2.00 | 2.50 | 3.00 |
| Compressive strength at 10% strain | ASTM-D3575 | 17 | 21 | 26 | 30 | 40 | 50 |
| Tensile strength at break | ASTM-D3575 | 34.3 | 44.4 | 52.9 | 60.3 | 72.6 | 82.6 |
| Tear strength at maximum load | ASTM-D3575 | 7.8 | 10.4 | 12.6 | 14.5 | 17.7 | 20.3 |
| Flexural strength at stress of 5% | ASTM-C203 | 26.9 | 37.5 | 47.5 | 57.0 | 74.2 | 89.2 |
| Bending stress at maximum cutting load | ASTM-C203 | 30.7 | 41.3 | 51.2 | 60.7 | 78.1 | 93.5 |
| Bending strain at maximum load | ASTM-C203 | 10.5 | 10.2 | 9.9 | 9.6 | 9.0 | 8.4 |
| puncture strength, maximum load | ASTM-D3763 | 38 | 47 | 56 | 65 | 83 | 101 |
| burn rate | FMVSS302 | 120.2 | 103.6 | 91.3 | 80.2 | 68.2 | 58.8 |
| thermal resistance | ASTMC518 | 3.79 | 3.87 | 3.92 | 3.97 | 4.01 | 4.01 |